Cation disorder dominates the defect chemistry of high-voltage LiMn <sub>1.5</sub> Ni <sub>0.5</sub> O <sub>4</sub> (LMNO) spinel cathodesJiayi Cen, David O. Scanlon, Alexander G. Squires et al.|Journal of Materials Chemistry A|2023Cited by 36
Li‐Site Defects Induce Formation of Li‐Rich Impurity Phases: Implications for Charge Distribution and Performance of LiNi<sub>0.5−</sub><i><sub>x</sub></i>M<i><sub>x</sub></i>Mn<sub>1.5</sub>O<sub>4</sub> Cathodes (M = Fe and Mg; <i>x</i> = 0.05–0.2)Beth E. Murdock, Nuria Tapia‐Ruiz, Seán R. Kavanagh et al.|Advanced Materials|2024Cited by 10
Cation disorder dominates the defect chemistry of high-voltage LiMn1.5Ni0.5O4 (LMNO) spinel cathodesJiayi Cen, David O. Scanlon, Bonan Zhu et al.|ChemRxiv|2023Cited by 3
Intrinsic Defect Chemistry of High-Voltage LiMn1.5Ni0.5O4 (LMNO) Spinel CathodeJiayi Cen, David O. Scanlon, Alexander G. Squires et al.|ChemRxiv|2023Cited by 2