An ultra-lithiophilic oxidation layer in a Ni-foam-based anode for lithium metal batteries
Yusong Choi(Korea National Defense University), Jang‐Hyeon Cho(Korea Advanced Institute of Science and Technology), Chi Hun Choi(Rice University), Tae-Ryong Park(Yuhan University), Sang-Hyeon Ha(Agency for Defense Development), Jae-In Lee(Yuhan University), Ji-Youn Kim(Yuhan University), Tae-Uk Hur(Yuhan University), Eun Hye Lee(Yuhan University), Tae–Young Ahn(Daejeon University)
Cited by 10
Related Papers
Battery metal recycling by flash Joule heating
|Science Advances|2023|120
Synthesis of Clean Hydrogen Gas from Waste Plastic at Zero Net Cost
|Advanced Materials|2023|89
Photoelectrochemical overall water splitting with textured CuBi <sub>2</sub> O <sub>4</sub> as a photocathode
|Chemical Communications|2018|88
Electrochemical properties of a lithium-impregnated metal foam anode for thermal batteries
|Journal of Power Sources|2014|54
Effect of the addition of carbon black and carbon nanotube to FeS2 cathode on the electrochemical performance of thermal battery
|Journal of Industrial and Engineering Chemistry|2013|54